Ultrasonic identification of weld defects made by electrofusion welding on plastic pipelines
ohlas Title statement Ultrasonic identification of weld defects made by electrofusion welding on plastic pipelines / aut. Martin Faturík, Miloš Mičian, Viera Zatkalíková, Ivo Hlavatý Main entry-name Faturík, Martin (Author) Another responsib. Mičian, Miloš (Author) Zatkalíková, Viera (Author) Hlavatý, Ivo (Author) In ERIN 2017. -- Ústí nad Labem : Univerzita J.E. Purkyně, 2017. -- ISBN 978-80-7561-056-0. -- S. 37-46 Language English Document kind RZB - článok zo zborníka References (1) - článok article