Corrosion behaviour of Ni-based superalloys in molten FLiNaK salts
Title statement Corrosion behaviour of Ni-based superalloys in molten FLiNaK salts / aut. Niketan S Patel, Viliam Pavlík, Blanka Kubíková, Martin Nosko, Vladimír Danielik, Miroslav Boča Main entry-name Patel, Niketan S. (Author) Another responsib. Pavlík, Viliam (Author) Kubíková, Blanka (Author) Nosko, Martin (Author) Danielik, Vladimír, 1968- Z1 (Author) - FCHPT Oddelenie anorganickej technológie Boča, Miroslav (Author) In Corrosion engineering science and technology. -- ISSN 1478-422X. -- Vol. 54, iss. 1 (2019), s. 46-53 Language English Document kind RBX - článok z periodika Category ADM - 13/NOVÉ Vedecké práce v zahraničných časopisoch registrovaných v databázach Web of Science alebo SCOPUS Category (from 2022) V3 - Vedecký výstup publikačnej činnosti z časopisu In databases WOS: 000454770400006
DOI: 10.1080/1478422X.2018.1525829Year 2019 article